NEXTREMA® Opaque Grey (712-8) Sheet

Want to keep this datasheet? Save it now in your required format

Description

NEXTREMA® is a unique glass-ceramic material platform. This material combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties like an attractive bending strength of 100 - 165 MPa for materials with a thickness of around 4 mm. With a thermal resistance of up to 950 °C, depending on the material type, combined with a thermal shock resistance of 600 - 820 °C, it ensures a reliable material performance even under extreme temperature conditions. Our six unique glass-ceramic types combined with the wide range of sizes and thicknesses varying from 2 mm to 6 mm (> 6 mm on request) will open up new possibilities in product design and performance. The unique transmission spectra provide new ideas for combining innovative infrared heating functionalities with attractive lighting effects. The versatility of this material will surely impress you. In addition, NEXTREMA® opaque grey (712-8) offers the highest maximum temperature resistance of up to 950 °C (1,742 °F) and the highest thermal insulation properties of all NEXTREMA® types due to lowest overall transmission in IR range.

This material data has been provided by SCHOTT AG.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperatureComment

Density

2.5 - 2.6 g/cm³

Show Supplier Material materials with Density of 2.5 - 2.6 g/cm³ at 20.0 °C

20.0 °C

approx.

Porosity

0 %

Show Supplier Material materials with Porosity of 0 %

approx., ISO 9385

Dimension

PropertyValue

Dimensions

Flat cut-to-size panels and bent panels are also available. Formats of flat cut-to-size panels and bent panels on request.

Length

1600 - 1954 mm

Show Supplier Material materials with Length of 1600 - 1954 mm

Thickness

3 - 6 mm

Show Supplier Material materials with Thickness of 3 - 6 mm

Width

900 - 1100 mm

Show Supplier Material materials with Width of 900 - 1100 mm

Mechanical

PropertyValueTemperatureComment

Elastic modulus

84 - 95 GPa

Show Supplier Material materials with Elastic modulus of 84 - 95 GPa at 20.0 °C

20.0 °C

approx., ASTM C-1259

Flexural strength

100 - 165 MPa

Show Supplier Material materials with Flexural strength of 100 - 165 MPa at 20.0 °C

20.0 °C

approx., DIN EN 1288, Part 5, R45

Hardness, Knoop, HK2

570 - 600 [-]

Show Supplier Material materials with Hardness, Knoop, HK2 of 570 - 600 [-] at 20.0 °C

20.0 °C

approx., ISO 9385 (HK 0.1/20)

Poisson's ratio

0.25 - 0.26 [-]

Show Supplier Material materials with Poisson's ratio of 0.25 - 0.26 [-] at 20.0 °C

20.0 °C

approx., ASTM C-1259

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

-8E-7 - 6E-7 1/K

Show Supplier Material materials with Coefficient of thermal expansion of -8E-7 - 6E-7 1/K at 50.0 °C

50.0 °C

for 0-50°C, DIN ISO 51045-1, DIN ISO 7991

Max service temperature

950 °C

Show Supplier Material materials with Max service temperature of 950 °C

short heating (1h) hom.

Specific heat capacity

800 - 850 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 800 - 850 J/(kg·K) at 20.0 °C

20.0 °C

for 20-100°C

Thermal conductivity

1.5 - 1.7 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 1.5 - 1.7 W/(m·K) at 90.0 °C

90.0 °C

DIN 51936, ASTM E 1461-01

Electrical

PropertyValueTemperatureComment

Dielectric constant, 1MHz

6.5 - 7.8 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 6.5 - 7.8 [-] at 25.0 °C

25.0 °C

DIN 53483

Electrical resistivity

3.98E+6 - 1.58E+7 Ω·m

Show Supplier Material materials with Electrical resistivity of 3.98E+6 - 1.58E+7 Ω·m at 250.0 °C

250.0 °C

DIN 52326

158489 - 501187 Ω·m

Show Supplier Material materials with Electrical resistivity of 158489 - 501187 Ω·m at 350.0 °C

350.0 °C

DIN 52326

Loss tangent

0 - 0.02 [-]

Show Supplier Material materials with Loss tangent of 0 - 0.02 [-] at 25.0 °C

25.0 °C

1MHz, DIN 53483

Acoustical

PropertyValueTemperatureComment

Sound speed, longitudinal

6300 - 6700 m/s

Show Supplier Material materials with Sound speed, longitudinal of 6300 - 6700 m/s at 20.0 °C

20.0 °C

ASTM C-1259

Chemical properties

Property

Aluminium

15 - 27 %

Al₂O₃ (DIN EN 1748-2-1)

Barium

0 - 8 %

BaO (DIN EN 1748-2-1)

Calcium

0 - 8 %

CaO (DIN EN 1748-2-1)

Lithium

0 - 5 %

Li₂O (DIN EN 1748-2-1)

Magnesium

0 - 8 %

MgO (DIN EN 1748-2-1)

Other

0 - 5 %

(DIN EN 1748-2-1)

Potassium

0 - 2 %

K₂O (DIN EN 1748-2-1)

Silicon

50 - 80 %

SiO₂ (DIN EN 1748-2-1)

Sodium

0 - 2 %

Na₂O (DIN EN 1748-2-1)

Titanium

0 - 5 %

TiO₂ (DIN EN 1748-2-1)

Zinc

0 - 5 %

ZnO (DIN EN 1748-2-1)

Zirconium

0 - 5 %

ZrO₂ (DIN EN 1748-2-1)

Technological properties

Property
Application areas

The following applications are simply examples of areas where NEXTREMA® has already been put to use successfully: BBQ applications - NEXTREMA® provides perfect visibility into the grill and can be used to optimize diverse aspects of the barbecue experience; IR applications - NEXTREMA® transforms infrared heaters into eye-catching design features and protects heating elements stylishly; High temperature furnaces - Use NEXTREMA® to line ovens or apply support plates (e.g. in display manufacturing); Household appliances - NEXTREMA® revolutionizes designs for transparent heating elements and heat resistant thin film coatings; Functional design material - NEXTREMA® is a revolutionary material for innovative product and industry design.

Compliance

NEXTREMA® materials do not contain any harmful substances according to the European directive 2002/95/EC “Hazardous Substances in electrical and electronically Equipment” and fulfill the terms of RoHS without any concerns.

Corrosion properties

The chemical resistance of NEXTREMA® is more extensive than that of most other comparable materials: Acid resistance (DIN 12116) S 1-2; Alkaline resistance (ISO 695) A 1-2; Hydrolytic class (DIN ISO 719) HGB 1.

Processing methods

NEXTREMA® is practically process inert. Even under extreme conditions, the material will not have negative interactions with the process environment. There are no interfering process factors such as gas emissions from organic components.