Boron Nitride (c-BN)

Want to keep this datasheet? Save it now in your required format

Description

Boron nitride is a chemical compound with equal numbers of boron and nitrogen atoms. The cubic (CBN) variety analogous to diamond has high hardness which is inferior only to diamond.

This material data has been provided by Advanced Ceramic Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

3.45 g/cm³

Show Supplier Material materials with Density of 3.45 g/cm³

Chemical properties

PropertyValueComment

Boron

40 - 41.9 %

Show Supplier Material materials with Boron of 40 - 41.9 %

Calcium

0.2 - 2 %

Show Supplier Material materials with Calcium of 0.2 - 2 %

Nitrogen

50 - 58.3 %

Show Supplier Material materials with Nitrogen of 50 - 58.3 %

Other

0.2 - 0.3 %

Show Supplier Material materials with Other of 0.2 - 0.3 %

Chloride, Iron, Aluminum, Silicon

Oxygen

0.3 - 3 %

Show Supplier Material materials with Oxygen of 0.3 - 3 %