EN 1753 MgAl9Zn1(A)

Want to keep this datasheet? Save it now in your required format

Primary standard name

This material data has been provided by Alu Key.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

8.3 - 9.7 %

Show Material materials with Aluminium of 8.3 - 9.7 %

Copper

0.03 %

Show Material materials with Copper of 0.03 %

Iron

5E-3 %

Show Material materials with Iron of 5E-3 %

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Nickel

1E-3 %

Show Material materials with Nickel of 1E-3 %

Silicon

0.2 %

Show Material materials with Silicon of 0.2 %

Zinc

0.4 - 1 %

Show Material materials with Zinc of 0.4 - 1 %