Chemical properties

PropertyValue

Copper

0.03 %

Show Material materials with Copper of 0.03 %

Iron

0.01 %

Show Material materials with Iron of 0.01 %

Manganese

0.15 %

Show Material materials with Manganese of 0.15 %

Nickel

5E-3 %

Show Material materials with Nickel of 5E-3 %

Rare Earth Elements

2.5 - 4 %

Show Material materials with Rare Earth Elements of 2.5 - 4 %

Silicon

0.01 %

Show Material materials with Silicon of 0.01 %

Zinc

2 - 3 %

Show Material materials with Zinc of 2 - 3 %

Zirconium

0.4 - 1 %

Show Material materials with Zirconium of 0.4 - 1 %