Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
DIN 1729-1 MgAl8Zn
This material data has been provided by Alu Key.
All categories
Let us help you find the best supplier!
Magnesium Alloys: Types, Properties and Applications
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationChemical properties
Property | Value |
---|---|
Aluminium | 7.8 - 9.2 % Show Material materials with Aluminium of 7.8 - 9.2 % |
Copper | 0.05 % Show Material materials with Copper of 0.05 % |
Iron | 5E-3 % Show Material materials with Iron of 5E-3 % |
Manganese | 0.12 - 0.3 % Show Material materials with Manganese of 0.12 - 0.3 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |
Zinc | 0.2 - 0.8 % Show Material materials with Zinc of 0.2 - 0.8 % |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
CONTACT US
+49 89 262075200
Leopoldstraße 250 A, 80807 Munich
© 2022 Matmatch GmbH, All rights reserved.
Made with ❤️ in Munich!