ASTM B951 Grade WE54A

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.7 g/cm³

Show Material materials with Density of 1.7 g/cm³

Typical for Cast Rare Earth Grade

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

40 - 45 GPa

Show Material materials with Elastic modulus of 40 - 45 GPa

Typical for Cast Rare Earth Grade

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Magnesium

Shear modulus

23.0 °C

45 GPa

Show Material materials with Shear modulus of 45 GPa

Typical for Magnesium

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.6E-5 1/K

Typical for Cast Rare Earth Grade

Melting point

535 - 645 °C

Show Material materials with Melting point of 535 - 645 °C

Typical for Cast Rare Earth Grade

Specific heat capacity

23.0 °C

966 - 1050 J/(kg·K)

Show Material materials with Specific heat capacity of 966 - 1050 J/(kg·K)

Typical for Cast Rare Earth Grade

Thermal conductivity

23.0 °C

51 - 113 W/(m·K)

Show Material materials with Thermal conductivity of 51 - 113 W/(m·K)

Typical for Cast Rare Earth Grade

Chemical properties

PropertyValue

Copper

0.03 %

Show Material materials with Copper of 0.03 %

Lithium

0.2 %

Show Material materials with Lithium of 0.2 %

Manganese

0.03 - 0.15 %

Show Material materials with Manganese of 0.03 - 0.15 %

Neodymium

1.5 - 2 %

Show Material materials with Neodymium of 1.5 - 2 %

Nickel

5E-3 %

Show Material materials with Nickel of 5E-3 %

Other

each 0.20, total 0.30, Rest Mg, Other rare earth metals should in principle be heavy rare earths, such as gadolinium, dysprosium, erbium and ytterbium. Other rare earth elements are derived from yttrium, typically 80 % Yttrium and 20 % heavy rare earth metals.,total 0.30. Rest Mg, Other rare earth metals should in principle be heavy rare earths, such as gadolinium, dysprosium, erbium and ytterbium. Other rare earth elements are derived from yttrium, typically 80 % Yttrium and 20 % heavy rare earth metals.,each 0.2. Rest Mg, Other rare earth metals should in principle be heavy rare earths, such as gadolinium, dysprosium, erbium and ytterbium. Other rare earth elements are derived from yttrium, typically 80 % Yttrium and 20 % heavy rare earth metals.

Silicon

0.01 %

Show Material materials with Silicon of 0.01 %

Yttrium

4.75 - 5.5 %

Show Material materials with Yttrium of 4.75 - 5.5 %

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

Zirconium

0.3 - 1 %

Show Material materials with Zirconium of 0.3 - 1 %