General

PropertyTemperatureValueComment

Density

23.0 °C

11.34 g/cm³

Show Material materials with Density of 11.34 g/cm³

Typical for Pure/Low Alloyed Lead

Mechanical

PropertyTemperatureValueComment

Poisson's ratio

23.0 °C

0.4 [-]

Show Material materials with Poisson's ratio of 0.4 [-]

Typical for Pure/Low Alloyed Lead

Thermal

PropertyTemperatureValueComment

Melting point

327 °C

Show Material materials with Melting point of 327 °C

Typical for Pure/Low Alloyed Lead

Specific heat capacity

23.0 °C

112 - 134 J/(kg·K)

Show Material materials with Specific heat capacity of 112 - 134 J/(kg·K)

Typical for Pure/Low Alloyed Lead

Thermal conductivity

23.0 °C

34 - 35 W/(m·K)

Show Material materials with Thermal conductivity of 34 - 35 W/(m·K)

Typical for Pure/Low Alloyed Lead

Chemical properties

PropertyValue

Antimony

0.3 - 0.7 %

Show Material materials with Antimony of 0.3 - 0.7 %

Arsenic

0.01 %

Show Material materials with Arsenic of 0.01 %

Bismuth

0.05 %

Show Material materials with Bismuth of 0.05 %

Copper

5E-3 %

Show Material materials with Copper of 5E-3 %

Other

Other impurities: Total 0.1. Rest Pb,, The hardening of Pb-Sb alloys can be improved by arsenic, for semi-finished products 0.04 to 0.06 % As is recommended.

Silver

8E-3 %

Show Material materials with Silver of 8E-3 %

Tin

5E-3 %

Show Material materials with Tin of 5E-3 %

Zinc

1E-3 %

Show Material materials with Zinc of 1E-3 %