DIN 17640-1 Grade 2.3219

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

11.3 g/cm³

Show Material materials with Density of 11.3 g/cm³

Mechanical

PropertyTemperatureValue

Hardness, Brinell

23.0 °C

7 [-]

Show Material materials with Hardness, Brinell of 7 [-]

Thermal

PropertyTemperatureValueComment

Melting point

235 - 305 °C

Show Material materials with Melting point of 235 - 305 °C

Typical for Lead Antimony

Specific heat capacity

23.0 °C

130 - 159 J/(kg·K)

Show Material materials with Specific heat capacity of 130 - 159 J/(kg·K)

Typical for Lead Antimony

Thermal conductivity

23.0 °C

24 - 34 W/(m·K)

Show Material materials with Thermal conductivity of 24 - 34 W/(m·K)

Typical for Lead Antimony

Chemical properties

PropertyValue

Antimony

1.8 - 2.2 %

Show Material materials with Antimony of 1.8 - 2.2 %

Arsenic

0.05 %

Show Material materials with Arsenic of 0.05 %

Bismuth

0.05 %

Show Material materials with Bismuth of 0.05 %

Cadmium

1E-3 %

Show Material materials with Cadmium of 1E-3 %

Copper

5E-3 %

Show Material materials with Copper of 5E-3 %

Other

Other impurities: Total 0.1. individually 0.03. Rest Pb., The age hardening of Pb-Sb alloys can be improved by arsenic, for casting alloys 0.08 to 0.15 % As are recommended.

Silver

8E-3 %

Show Material materials with Silver of 8E-3 %