EN 12548 Grade PB022K

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyTemperatureValueComment

Melting point

185 - 320 °C

Show Material materials with Melting point of 185 - 320 °C

Typical for Lead Tin

Specific heat capacity

23.0 °C

213 - 239 J/(kg·K)

Show Material materials with Specific heat capacity of 213 - 239 J/(kg·K)

Typical for Lead Tin

Thermal conductivity

23.0 °C

35 - 57 W/(m·K)

Show Material materials with Thermal conductivity of 35 - 57 W/(m·K)

Typical for Lead Tin

Chemical properties

PropertyValue

Antimony

0.06 - 0.1 %

Show Material materials with Antimony of 0.06 - 0.1 %

Arsenic

1E-3 %

Show Material materials with Arsenic of 1E-3 %

Bismuth

0.03 %

Show Material materials with Bismuth of 0.03 %

Cadmium

1E-3 %

Show Material materials with Cadmium of 1E-3 %

Copper

3E-3 %

Show Material materials with Copper of 3E-3 %

Nickel

1E-3 %

Show Material materials with Nickel of 1E-3 %

Other

Rest Pb

Silver

5E-3 %

Show Material materials with Silver of 5E-3 %

Tellurium

2E-3 %

Show Material materials with Tellurium of 2E-3 %

Tin

0.35 - 0.45 %

Show Material materials with Tin of 0.35 - 0.45 %

Zinc

5E-4 %

Show Material materials with Zinc of 5E-4 %