EN 12548 Grade PB051K

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

11.34 g/cm³

Show Material materials with Density of 11.34 g/cm³

Typical for Pure/Low Alloyed Lead

Mechanical

PropertyTemperatureValueComment

Poisson's ratio

23.0 °C

0.4 [-]

Show Material materials with Poisson's ratio of 0.4 [-]

Typical for Pure/Low Alloyed Lead

Thermal

PropertyTemperatureValueComment

Melting point

327 °C

Show Material materials with Melting point of 327 °C

Typical for Pure/Low Alloyed Lead

Specific heat capacity

23.0 °C

112 - 134 J/(kg·K)

Show Material materials with Specific heat capacity of 112 - 134 J/(kg·K)

Typical for Pure/Low Alloyed Lead

Thermal conductivity

23.0 °C

34 - 35 W/(m·K)

Show Material materials with Thermal conductivity of 34 - 35 W/(m·K)

Typical for Pure/Low Alloyed Lead

Chemical properties

PropertyValue

Antimony

1E-3 %

Show Material materials with Antimony of 1E-3 %

Arsenic

1E-3 %

Show Material materials with Arsenic of 1E-3 %

Bismuth

0.015 %

Show Material materials with Bismuth of 0.015 %

Cadmium

1E-3 %

Show Material materials with Cadmium of 1E-3 %

Calcium

0.02 - 0.04 %

Show Material materials with Calcium of 0.02 - 0.04 %

Copper

1E-3 %

Show Material materials with Copper of 1E-3 %

Nickel

5E-4 %

Show Material materials with Nickel of 5E-4 %

Other

Rest Pb

Silver

2.5E-3 %

Show Material materials with Silver of 2.5E-3 %

Tellurium

2E-3 %

Show Material materials with Tellurium of 2E-3 %

Tin

0.3 - 0.4 %

Show Material materials with Tin of 0.3 - 0.4 %

Zinc

5E-4 %

Show Material materials with Zinc of 5E-4 %