DIN 1742 Grade 2.3722

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.9 g/cm³

Show Material materials with Density of 7.9 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

1.7 %

Show Material materials with Elongation of 1.7 %

Hardness, Brinell

23.0 °C

28 [-]

Show Material materials with Hardness, Brinell of 28 [-]

Tensile strength

23.0 °C

90 MPa

Show Material materials with Tensile strength of 90 MPa

Thermal

PropertyTemperatureValueComment

Melting point

215 - 350 °C

Show Material materials with Melting point of 215 - 350 °C

Typical for Tin Antimony

Thermal conductivity

23.0 °C

40 W/(m·K)

Show Material materials with Thermal conductivity of 40 W/(m·K)

Typical for Tin Antimony

Chemical properties

PropertyValue

Aluminium

0.01 %

Show Material materials with Aluminium of 0.01 %

Antimony

12 - 14 %

Show Material materials with Antimony of 12 - 14 %

Arsenic

0.08 %

Show Material materials with Arsenic of 0.08 %

Copper

2 - 3 %

Show Material materials with Copper of 2 - 3 %

Iron

0.08 %

Show Material materials with Iron of 0.08 %

Other

Rest Pb

Tin

59 - 61 %

Show Material materials with Tin of 59 - 61 %

Zinc

0.01 %

Show Material materials with Zinc of 0.01 %