DIN 1707-100 Grade S-Sn90Pb10

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.7 g/cm³

Show Material materials with Density of 7.7 g/cm³

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.1E-5 - 2.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.1E-5 - 2.9E-5 1/K

Typical for Tin Lead

Melting point

183 - 215 °C

Show Material materials with Melting point of 183 - 215 °C

Specific heat capacity

23.0 °C

150 - 239 J/(kg·K)

Show Material materials with Specific heat capacity of 150 - 239 J/(kg·K)

Typical for Tin Lead

Thermal conductivity

23.0 °C

46 - 57 W/(m·K)

Show Material materials with Thermal conductivity of 46 - 57 W/(m·K)

Typical for Tin Lead

Chemical properties

PropertyValue

Aluminium

1E-3 %

Show Material materials with Aluminium of 1E-3 %

Antimony

0.2 %

Show Material materials with Antimony of 0.2 %

Arsenic

0.03 %

Show Material materials with Arsenic of 0.03 %

Bismuth

0.1 %

Show Material materials with Bismuth of 0.1 %

Cadmium

1E-3 %

Show Material materials with Cadmium of 1E-3 %

Copper

0.08 %

Show Material materials with Copper of 0.08 %

Gold

0.05 %

Show Material materials with Gold of 0.05 %

Indium

0.1 %

Show Material materials with Indium of 0.1 %

Iron

0.02 %

Show Material materials with Iron of 0.02 %

Nickel

0.01 %

Show Material materials with Nickel of 0.01 %

Other

Rest Pb

Silver

0.1 %

Show Material materials with Silver of 0.1 %

Tin

89.5 - 90.5 %

Show Material materials with Tin of 89.5 - 90.5 %

Zinc

1E-3 %

Show Material materials with Zinc of 1E-3 %