EN 1774 Grade ZL5

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

5 g/cm³

Show Material materials with Density of 5 g/cm³

Typical for Zinc Aluminium

Mechanical

PropertyTemperatureValueComment

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Zinc Aluminium

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.2E-5 - 2.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K

Typical for Zinc Aluminium

Melting point

375 - 485 °C

Show Material materials with Melting point of 375 - 485 °C

Typical for Zinc Aluminium

Specific heat capacity

23.0 °C

393 - 525 J/(kg·K)

Show Material materials with Specific heat capacity of 393 - 525 J/(kg·K)

Typical for Zinc Aluminium

Thermal conductivity

23.0 °C

105 - 125 W/(m·K)

Show Material materials with Thermal conductivity of 105 - 125 W/(m·K)

Typical for Zinc Aluminium

Chemical properties

PropertyValue

Aluminium

3.8 - 4.2 %

Show Material materials with Aluminium of 3.8 - 4.2 %

Cadmium

3E-3 %

Show Material materials with Cadmium of 3E-3 %

Copper

0.7 - 1.1 %

Show Material materials with Copper of 0.7 - 1.1 %

Iron

0.02 %

Show Material materials with Iron of 0.02 %

Lead

3E-3 %

Show Material materials with Lead of 3E-3 %

Magnesium

0.04 - 0.06 %

Show Material materials with Magnesium of 0.04 - 0.06 %

Nickel

1E-3 %

Show Material materials with Nickel of 1E-3 %

Other

Rest Zn

Silicon

0.02 %

Show Material materials with Silicon of 0.02 %

Tin

1E-3 %

Show Material materials with Tin of 1E-3 %