ISO 17672 Grade Ni 600

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyValue

Melting point

980 - 1060 °C

Show Material materials with Melting point of 980 - 1060 °C

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Boron

2.75 - 3.5 %

Show Material materials with Boron of 2.75 - 3.5 %

Cadmium

0.01 %

Show Material materials with Cadmium of 0.01 %

Carbon

0.6 - 0.9 %

Show Material materials with Carbon of 0.6 - 0.9 %

Chromium

13 - 15 %

Show Material materials with Chromium of 13 - 15 %

Cobalt

0.1 %

Show Material materials with Cobalt of 0.1 %

Iron

4 - 5 %

Show Material materials with Iron of 4 - 5 %

Lead

0.03 %

Show Material materials with Lead of 0.03 %

Other

Andere Beimengungen: zusammen 0,50, Rest Ni

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Selenium

5E-3 %

Show Material materials with Selenium of 5E-3 %

Silicon

4 - 5 %

Show Material materials with Silicon of 4 - 5 %

Sulfur

0.02 %

Show Material materials with Sulfur of 0.02 %

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

Zirconium

0.05 %

Show Material materials with Zirconium of 0.05 %