DIN 1701 Grade 2.4011

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Typical for Pure/Low Nickel Alloy

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 220 GPa

Show Material materials with Elastic modulus of 190 - 220 GPa

Typical for Pure/Low Nickel Alloy

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

8.5E-6 - 1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 8.5E-6 - 1.4E-5 1/K

Typical for Pure/Low Nickel Alloy

Melting point

1400 - 1500 °C

Show Material materials with Melting point of 1400 - 1500 °C

Typical for Pure/Low Nickel Alloy

Specific heat capacity

23.0 °C

430 - 532 J/(kg·K)

Show Material materials with Specific heat capacity of 430 - 532 J/(kg·K)

Typical for Pure/Low Nickel Alloy

Thermal conductivity

23.0 °C

18 - 86 W/(m·K)

Show Material materials with Thermal conductivity of 18 - 86 W/(m·K)

Typical for Pure/Low Nickel Alloy

Chemical properties

PropertyValue

Antimony

1E-4 %

Show Material materials with Antimony of 1E-4 %

Arsenic

1E-3 %

Show Material materials with Arsenic of 1E-3 %

Bismuth

1E-4 %

Show Material materials with Bismuth of 1E-4 %

Carbon

0.015 %

Show Material materials with Carbon of 0.015 %

Cobalt

0.01 %

Show Material materials with Cobalt of 0.01 %

Copper

5E-3 %

Show Material materials with Copper of 5E-3 %

Iron

0.02 %

Show Material materials with Iron of 0.02 %

Lead

5E-4 %

Show Material materials with Lead of 5E-4 %

Manganese

5E-4 %

Show Material materials with Manganese of 5E-4 %

Nickel

99.96 %

Show Material materials with Nickel of 99.96 %

Other

The nickel composition includes Co

Phosphorus

1E-3 %

Show Material materials with Phosphorus of 1E-3 %

Selenium

2E-4 %

Show Material materials with Selenium of 2E-4 %

Silver

5E-4 %

Show Material materials with Silver of 5E-4 %

Sulfur

1.5E-3 %

Show Material materials with Sulfur of 1.5E-3 %

Tantalum

5E-4 %

Show Material materials with Tantalum of 5E-4 %

Tellurium

1E-4 %

Show Material materials with Tellurium of 1E-4 %

Thallium

1E-4 %

Show Material materials with Thallium of 1E-4 %

Tin

1E-4 %

Show Material materials with Tin of 1E-4 %

Zinc

1E-3 %

Show Material materials with Zinc of 1E-3 %