ISO 6283 Grade Ni 9995

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Antimony

1E-3 %

Show Material materials with Antimony of 1E-3 %

Arsenic

1E-3 %

Show Material materials with Arsenic of 1E-3 %

Bismuth

5E-4 %

Show Material materials with Bismuth of 5E-4 %

Carbon

0.015 %

Show Material materials with Carbon of 0.015 %

Cobalt

0.1 %

Show Material materials with Cobalt of 0.1 %

Copper

5E-3 %

Show Material materials with Copper of 5E-3 %

Iron

0.02 %

Show Material materials with Iron of 0.02 %

Lead

1E-3 %

Show Material materials with Lead of 1E-3 %

Nickel

99.95 %

Show Material materials with Nickel of 99.95 %

Other

The nickel composition includes Co

Phosphorus

2E-3 %

Show Material materials with Phosphorus of 2E-3 %

Selenium

1E-3 %

Show Material materials with Selenium of 1E-3 %

Silver

5E-4 %

Show Material materials with Silver of 5E-4 %

Sulfur

2.5E-3 %

Show Material materials with Sulfur of 2.5E-3 %

Tellurium

5E-4 %

Show Material materials with Tellurium of 5E-4 %

Thallium

5E-4 %

Show Material materials with Thallium of 5E-4 %

Tin

5E-4 %

Show Material materials with Tin of 5E-4 %

Zinc

2E-3 %

Show Material materials with Zinc of 2E-3 %