ISO 18274 Grade Ni 6045

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

0.3 %

Show Material materials with Aluminium of 0.3 %

Carbon

0.05 - 0.12 %

Show Material materials with Carbon of 0.05 - 0.12 %

Chromium

26 - 29 %

Show Material materials with Chromium of 26 - 29 %

Cobalt

1 %

Show Material materials with Cobalt of 1 %

Copper

0.3 %

Show Material materials with Copper of 0.3 %

Iron

21 - 25 %

Show Material materials with Iron of 21 - 25 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

40 %

Show Material materials with Nickel of 40 %

Other

total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt.

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

2.5 - 3 %

Show Material materials with Silicon of 2.5 - 3 %

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %