Chemical properties

PropertyValue

Aluminium

0.2 %

Show Material materials with Aluminium of 0.2 %

Carbon

0.02 %

Show Material materials with Carbon of 0.02 %

Chromium

23 - 27 %

Show Material materials with Chromium of 23 - 27 %

Copper

1.5 - 3 %

Show Material materials with Copper of 1.5 - 3 %

Iron

30 %

Show Material materials with Iron of 30 %

Manganese

1 - 3 %

Show Material materials with Manganese of 1 - 3 %

Molybdenum

3.5 - 7.5 %

Show Material materials with Molybdenum of 3.5 - 7.5 %

Nickel

37 - 42 %

Show Material materials with Nickel of 37 - 42 %

Other

total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt.

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

1 %

Show Material materials with Titanium of 1 %