Chemical properties

PropertyValue

Aluminium

0.8 - 1.5 %

Show Material materials with Aluminium of 0.8 - 1.5 %

Carbon

0.05 - 0.15 %

Show Material materials with Carbon of 0.05 - 0.15 %

Chromium

20 - 24 %

Show Material materials with Chromium of 20 - 24 %

Cobalt

10 - 15 %

Show Material materials with Cobalt of 10 - 15 %

Copper

0.5 %

Show Material materials with Copper of 0.5 %

Iron

3 %

Show Material materials with Iron of 3 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

8 - 10 %

Show Material materials with Molybdenum of 8 - 10 %

Nickel

44 %

Show Material materials with Nickel of 44 %

Other

total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt.

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

0.6 %

Show Material materials with Titanium of 0.6 %

Tungsten

0.5 %

Show Material materials with Tungsten of 0.5 %