Chemical properties

PropertyValue

Aluminium

1 - 2 %

Show Material materials with Aluminium of 1 - 2 %

Bismuth

1E-4 %

Show Material materials with Bismuth of 1E-4 %

Boron

0.02 %

Show Material materials with Boron of 0.02 %

Carbon

0.13 %

Show Material materials with Carbon of 0.13 %

Chromium

18 - 21 %

Show Material materials with Chromium of 18 - 21 %

Cobalt

15 - 18 %

Show Material materials with Cobalt of 15 - 18 %

Copper

0.2 %

Show Material materials with Copper of 0.2 %

Iron

1.5 %

Show Material materials with Iron of 1.5 %

Lead

2E-3 %

Show Material materials with Lead of 2E-3 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

50 %

Show Material materials with Nickel of 50 %

Other

total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt.

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Silver

5E-4 %

Show Material materials with Silver of 5E-4 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

2 - 3 %

Show Material materials with Titanium of 2 - 3 %

Zirconium

0.15 %

Show Material materials with Zirconium of 0.15 %