ISO 14172 Grade Ni 6024

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Carbon

0.02 %

Show Material materials with Carbon of 0.02 %

Chromium

25 - 27 %

Show Material materials with Chromium of 25 - 27 %

Copper

0.5 %

Show Material materials with Copper of 0.5 %

Iron

1.5 %

Show Material materials with Iron of 1.5 %

Manganese

0.5 %

Show Material materials with Manganese of 0.5 %

Molybdenum

13.5 - 15 %

Show Material materials with Molybdenum of 13.5 - 15 %

Nickel

55 %

Show Material materials with Nickel of 55 %

Other

total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt.

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.2 %

Show Material materials with Silicon of 0.2 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %