Chemical properties

PropertyValue

Carbon

0.1 %

Show Material materials with Carbon of 0.1 %

Chromium

14.5 - 16.5 %

Show Material materials with Chromium of 14.5 - 16.5 %

Cobalt

2.5 %

Show Material materials with Cobalt of 2.5 %

Copper

0.5 %

Show Material materials with Copper of 0.5 %

Iron

4 - 7 %

Show Material materials with Iron of 4 - 7 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

15 - 18 %

Show Material materials with Molybdenum of 15 - 18 %

Nickel

50 %

Show Material materials with Nickel of 50 %

Other

total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt.

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Tungsten

3 - 4.5 %

Show Material materials with Tungsten of 3 - 4.5 %

Vanadium

0.4 %