Chemical properties

PropertyValue

Carbon

0.1 %

Show Material materials with Carbon of 0.1 %

Chromium

12 - 17 %

Show Material materials with Chromium of 12 - 17 %

Copper

0.5 %

Show Material materials with Copper of 0.5 %

Iron

10 %

Show Material materials with Iron of 10 %

Manganese

2 - 4 %

Show Material materials with Manganese of 2 - 4 %

Molybdenum

5 - 9 %

Show Material materials with Molybdenum of 5 - 9 %

Nickel

55 %

Show Material materials with Nickel of 55 %

Niobium

0.5 - 2 %

Show Material materials with Niobium of 0.5 - 2 %

Other

total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum.

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Tungsten

1 - 2 %