DIN 1707-100 Grade S-Cd68Zn22Ag10

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.4 g/cm³

Show Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

50 GPa

Show Material materials with Elastic modulus of 50 GPa

Typical for Cadmium

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Cadmium

Shear modulus

23.0 °C

19.2 GPa

Show Material materials with Shear modulus of 19.2 GPa

Typical for Cadmium

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

3E-5 - 3.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 3E-5 - 3.2E-5 1/K

Typical for Cadmium

Melting point

270 - 380 °C

Show Material materials with Melting point of 270 - 380 °C

Specific heat capacity

23.0 °C

230 J/(kg·K)

Show Material materials with Specific heat capacity of 230 J/(kg·K)

Typical for Cadmium

Thermal conductivity

23.0 °C

84 - 97 W/(m·K)

Show Material materials with Thermal conductivity of 84 - 97 W/(m·K)

Typical for Cadmium

Chemical properties

PropertyValue

Aluminium

1E-3 %

Show Material materials with Aluminium of 1E-3 %

Antimony

0.1 %

Show Material materials with Antimony of 0.1 %

Arsenic

0.03 %

Show Material materials with Arsenic of 0.03 %

Bismuth

0.1 %

Show Material materials with Bismuth of 0.1 %

Copper

0.1 %

Show Material materials with Copper of 0.1 %

Gold

0.05 %

Show Material materials with Gold of 0.05 %

Indium

0.1 %

Show Material materials with Indium of 0.1 %

Iron

0.02 %

Show Material materials with Iron of 0.02 %

Lead

0.1 %

Show Material materials with Lead of 0.1 %

Nickel

0.01 %

Show Material materials with Nickel of 0.01 %

Other

Rest Cd

Silver

9.5 - 10.5 %

Show Material materials with Silver of 9.5 - 10.5 %

Tin

0.1 %

Show Material materials with Tin of 0.1 %

Zinc

21 - 23 %

Show Material materials with Zinc of 21 - 23 %