General
Property | Value | Condition | Related Standards |
---|---|---|---|
Density | 2.75 g/cm³ Show Material materials with Density of 2.75 g/cm³ | T64 | EN 1706 |
Mechanical
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | T64 | EN 1706 | |
Elastic modulus | 72.0 GPa Show Material materials with Elastic modulus of 72.0 GPa | T64 | EN 1706 | |
Hardness, Brinell | 85.0 [-] Show Material materials with Hardness, Brinell of 85.0 [-] | T64 | EN 1706 | |
90.0 [-] Show Material materials with Hardness, Brinell of 90.0 [-] | T64 | EN 1706 | ||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | ||
Tensile strength | 280.0 MPa Show Material materials with Tensile strength of 280.0 MPa | T64 | EN 1706 | |
320.0 MPa Show Material materials with Tensile strength of 320.0 MPa | T64 | EN 1706 |
Thermal
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.3e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3e-05 1/K | T64 | EN 1706 |
100 °C | 2.3e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3e-05 1/K | T64 | EN 1706 | |
Melting point | 540.0 - 640.0 °C Show Material materials with Melting point of 540.0 - 640.0 °C | T64 | EN 1706 | |
Specific heat capacity | 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 J/(kg·K) | T64 | EN 1706 | |
Thermal conductivity | 120.0 - 150.0 W/(m·K) Show Material materials with Thermal conductivity of 120.0 - 150.0 W/(m·K) | T64 | EN 1706 |
Electrical
Property | Value | Condition | Related Standards |
---|---|---|---|
Electrical conductivity | 16000000.0 - 23000000.0 S/m Show Material materials with Electrical conductivity of 16000000.0 - 23000000.0 S/m | T64 | EN 1706 |
Electrical resistivity | 4.35e-08 - 6.25e-08 Ω·m Show Material materials with Electrical resistivity of 4.35e-08 - 6.25e-08 Ω·m | T64 | EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Copper | 4.5 - 5.2 % Show Material materials with Copper of 4.5 - 5.2 % | T64 | EN 1706 |
Iron | 0.18 % Show Material materials with Iron of 0.18 % | T64 | EN 1706 |
Manganese | 0.001 - 0.5 % Show Material materials with Manganese of 0.001 - 0.5 % | T64 | EN 1706 |
Silicon | 0.18 % Show Material materials with Silicon of 0.18 % | T64 | EN 1706 |
Titanium | 0.15 % Show Material materials with Titanium of 0.15 % | T64 | EN 1706 |
Zinc | 0.07 % Show Material materials with Zinc of 0.07 % | T64 | EN 1706 |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: acceptable | |
Corrosion properties | general: not sufficient | |
General machinability | as cast: excellent |