General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 11.34 g/cm³ Show Material materials with Density of 11.34 g/cm³ | Typical for Pure/Low Alloyed Lead |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Poisson's ratio | 23.0 °C | 0.4 [-] Show Material materials with Poisson's ratio of 0.4 [-] | Typical for Pure/Low Alloyed Lead |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 327 °C Show Material materials with Melting point of 327 °C | Typical for Pure/Low Alloyed Lead | |
Specific heat capacity | 23.0 °C | 112 - 134 J/(kg·K) Show Material materials with Specific heat capacity of 112 - 134 J/(kg·K) | Typical for Pure/Low Alloyed Lead |
Thermal conductivity | 23.0 °C | 34 - 35 W/(m·K) Show Material materials with Thermal conductivity of 34 - 35 W/(m·K) | Typical for Pure/Low Alloyed Lead |
Chemical properties
Property | Value |
---|---|
Antimony | 1E-3 % Show Material materials with Antimony of 1E-3 % |
Arsenic | 1E-3 % Show Material materials with Arsenic of 1E-3 % |
Bismuth | 0.06 % Show Material materials with Bismuth of 0.06 % |
Cadmium | 2E-3 % Show Material materials with Cadmium of 2E-3 % |
Copper | 5E-3 % Show Material materials with Copper of 5E-3 % |
Lead | 99.94 % Show Material materials with Lead of 99.94 % |
Nickel | 2E-3 % Show Material materials with Nickel of 2E-3 % |
Other | Other impurities: Total 0.060 |
Silver | 8E-3 % Show Material materials with Silver of 8E-3 % |
Tin | 1E-3 % Show Material materials with Tin of 1E-3 % |
Zinc | 5E-4 % Show Material materials with Zinc of 5E-4 % |