General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.2 g/cm³ Show Material materials with Density of 7.2 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 105 GPa Show Material materials with Elastic modulus of 105 GPa | Typical for Zinc |
Elongation A50 | 23.0 °C | 35 % Show Material materials with Elongation A50 of 35 % | |
Poisson's ratio | 23.0 °C | 0.25 [-] Show Material materials with Poisson's ratio of 0.25 [-] | Typical for Zinc |
Shear modulus | 23.0 °C | 42 GPa Show Material materials with Shear modulus of 42 GPa | Typical for Zinc |
Tensile strength | 23.0 °C | 150 MPa Show Material materials with Tensile strength of 150 MPa | |
Yield strength Rp0.2 | 23.0 °C | 100 MPa Show Material materials with Yield strength Rp0.2 of 100 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 2.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.2E-5 1/K | |
Melting point | 420 °C Show Material materials with Melting point of 420 °C | ||
Specific heat capacity | 23.0 °C | 272 - 525 J/(kg·K) Show Material materials with Specific heat capacity of 272 - 525 J/(kg·K) | Typical for Zinc |
Thermal conductivity | 23.0 °C | 110 W/(m·K) Show Material materials with Thermal conductivity of 110 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.70E+7 S/m Show Material materials with Electrical conductivity of 1.70E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.015 % Show Material materials with Aluminium of 0.015 % |
Copper | 0.08 - 1 % Show Material materials with Copper of 0.08 - 1 % |
Other | Rest Zn |
Titanium | 0.06 - 0.2 % Show Material materials with Titanium of 0.06 - 0.2 % |