General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.2 g/cm³ Show Material materials with Density of 7.2 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Melting point | 375 - 485 °C Show Material materials with Melting point of 375 - 485 °C | Typical for Zinc Aluminium | |
Specific heat capacity | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Specific heat capacity of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Thermal conductivity | 20.0 °C | 109 W/(m·K) Show Material materials with Thermal conductivity of 109 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 1.39E+7 S/m Show Material materials with Electrical conductivity of 1.39E+7 S/m |
Electrical resistivity | 20.0 °C | 7.2E-8 Ω·m Show Material materials with Electrical resistivity of 7.2E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 - 0.04 % Show Material materials with Aluminium of 0.01 - 0.04 % |
Cadmium | 5E-3 % Show Material materials with Cadmium of 5E-3 % |
Chromium | 0.1 - 0.2 % Show Material materials with Chromium of 0.1 - 0.2 % |
Copper | 1 - 1.5 % Show Material materials with Copper of 1 - 1.5 % |
Iron | 0.06 % Show Material materials with Iron of 0.06 % |
Lead | 5E-3 % Show Material materials with Lead of 5E-3 % |
Magnesium | 0.02 % Show Material materials with Magnesium of 0.02 % |
Other | Rest Zn |
Silicon | 0.05 % Show Material materials with Silicon of 0.05 % |
Tin | 4E-3 % Show Material materials with Tin of 4E-3 % |
Titanium | 0.15 - 0.25 % Show Material materials with Titanium of 0.15 - 0.25 % |
Zinc | 97.87 % Show Material materials with Zinc of 97.87 % |