Description

The material ZP2 with the material number ZP0430 is applied for sand and gravity die-castings of any kind, sheet-metal-forming tools as well as for moulds for injection-molding, deep-drawing and blowing of plastics. The alloy ZP2 is a possible alternative for the material ZP5 (ZP0410) if the strength of that material is insufficient. In the alloy family with 4 mass-per-cent aluminium, ZP2 possesses the highest strength and the best behaviour in terms of creep strength depending on time. According to DIN EN 12844, the alternating stress fatigue strength (time strength) is 60 N/mm² with 100 million reversals of stress, the creep life (0.5 per cent, 3000 h) is 130 N/mm². The temperature coefficient of the length is 27 µm/m*K.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

6.8 g/cm³

Show Material materials with Density of 6.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Bending Fatigue Strength

23.0 °C

60 MPa

Show Material materials with Bending Fatigue Strength of 60 MPa

Elastic modulus

20.0 °C

85 GPa

Show Material materials with Elastic modulus of 85 GPa

Elongation A50

20.0 °C

5 %

Show Material materials with Elongation A50 of 5 %

23.0 °C

5 %

Show Material materials with Elongation A50 of 5 %

Hardness, Brinell

20.0 °C

102 [-]

Show Material materials with Hardness, Brinell of 102 [-]

23.0 °C

102 [-]

Show Material materials with Hardness, Brinell of 102 [-]

Unlock all property charts

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Zinc Aluminium

Tensile strength

20.0 °C

335 MPa

Show Material materials with Tensile strength of 335 MPa

23.0 °C

335 MPa

Show Material materials with Tensile strength of 335 MPa

Unlock all property charts

Yield strength Rp0.2

20.0 °C

270 MPa

Show Material materials with Yield strength Rp0.2 of 270 MPa

23.0 °C

270 MPa

Show Material materials with Yield strength Rp0.2 of 270 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.2E-5 - 2.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K

Typical for Zinc Aluminium

Melting point

375 - 485 °C

Show Material materials with Melting point of 375 - 485 °C

Typical for Zinc Aluminium

Specific heat capacity

23.0 °C

393 - 525 J/(kg·K)

Show Material materials with Specific heat capacity of 393 - 525 J/(kg·K)

Typical for Zinc Aluminium

Thermal conductivity

20.0 °C

119 W/(m·K)

Show Material materials with Thermal conductivity of 119 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

1.51E+7 S/m

Show Material materials with Electrical conductivity of 1.51E+7 S/m

Electrical resistivity

20.0 °C

6.6E-8 Ω·m

Show Material materials with Electrical resistivity of 6.6E-8 Ω·m

Chemical properties

PropertyValue

Aluminium

3.7 - 4.3 %

Show Material materials with Aluminium of 3.7 - 4.3 %

Cadmium

5E-3 %

Show Material materials with Cadmium of 5E-3 %

Copper

2.7 - 3.3 %

Show Material materials with Copper of 2.7 - 3.3 %

Iron

0.05 %

Show Material materials with Iron of 0.05 %

Lead

5E-3 %

Show Material materials with Lead of 5E-3 %

Magnesium

0.03 - 0.06 %

Show Material materials with Magnesium of 0.03 - 0.06 %

Nickel

0.02 %

Show Material materials with Nickel of 0.02 %

Other

Rest Zn

Silicon

0.03 %

Show Material materials with Silicon of 0.03 %

Tin

0 - 0.02 %

Show Material materials with Tin of 0 - 0.02 %

Zinc

92.23 %

Show Material materials with Zinc of 92.23 %