GOST 859 Grade M00 k

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Antimony

4E-4 %

Show Material materials with Antimony of 4E-4 %

Arsenic

5E-4 %

Show Material materials with Arsenic of 5E-4 %

Iron

1E-3 %

Show Material materials with Iron of 1E-3 %

Lead

5E-4 %

Show Material materials with Lead of 5E-4 %

Oxygen

0.01 %

Show Material materials with Oxygen of 0.01 %

Silver

2E-3 %

Show Material materials with Silver of 2E-3 %

Sulfur

1.5E-3 %

Show Material materials with Sulfur of 1.5E-3 %