5086 H18 Non-Heat Treatable Al Wrought Alloy

Want to keep this datasheet? Save it now in your required format

Description

High corrosion resistance against seawater.

Related Standards

Equivalent Materials

This material data has been provided by Aludium.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.66 g/cm³

Show Supplier Material materials with Density of 2.66 g/cm³

Dimension

PropertyValue

Thickness

0.2 - 3 mm

Show Supplier Material materials with Thickness of 0.2 - 3 mm

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

71 GPa

Show Supplier Material materials with Elastic modulus of 71 GPa

Elongation A50

23.0 °C

1 %

Show Supplier Material materials with Elongation A50 of 1 %

Hardness, HBW

23.0 °C

104 [-]

Show Supplier Material materials with Hardness, HBW of 104 [-]

Shear modulus

23.0 °C

27 GPa

Show Supplier Material materials with Shear modulus of 27 GPa

Tensile strength

23.0 °C

345 MPa

Show Supplier Material materials with Tensile strength of 345 MPa

Yield strength

23.0 °C

290 MPa

Show Supplier Material materials with Yield strength of 290 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

2.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.4E-5 1/K

20-100°C

Thermal conductivity

23.0 °C

126 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 126 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

5.6E-8 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.6E-8 Ω·m

Chemical properties

PropertyValue

Chromium

0.05 - 0.25 %

Show Supplier Material materials with Chromium of 0.05 - 0.25 %

Copper

0.1 %

Show Supplier Material materials with Copper of 0.1 %

Iron

0.5 %

Show Supplier Material materials with Iron of 0.5 %

Magnesium

3.5 - 4.5 %

Show Supplier Material materials with Magnesium of 3.5 - 4.5 %

Manganese

0.2 - 0.7 %

Show Supplier Material materials with Manganese of 0.2 - 0.7 %

Other

0.05 - 0.15 %

Show Supplier Material materials with Other of 0.05 - 0.15 %

Silicon

0.4 %

Show Supplier Material materials with Silicon of 0.4 %

Titanium

0.15 %

Show Supplier Material materials with Titanium of 0.15 %

Zinc

0.25 %

Show Supplier Material materials with Zinc of 0.25 %

Technological properties

Property
Anodizing

Excellent (anodizing quality)

Application areas

Vessels: Pressure, Cryogenics; Components: Access hatches, Spoilers, General tranportation

Corrosion properties

Excellent

Welding

Good

Workability

Good (in O temper)