PH 1.4542

Alternative and trade names
PH 17-4/630/1.4542
Want to keep this datasheet? Save it now in your required format

Description

Ambica’s 17-4 material offers following benefits:


High Tensile Strength and Toughness

Excellent Corrosion Resistance

Suitable for Forging and Welding

Good machinability

Good Oxidation Resistance

This product is available in the following forms: Bright round bars, Cold Drawn Hex / Square Bars, HRAP Square Bars, HRAP Flat Bars, Billets, Ingots.

Related Standards

Equivalent Materials

This material data has been provided by AMBI.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

12 %

Show Supplier Material materials with Elongation of 12 %

Hardness, HBW

23.0 °C

360 [-]

Show Supplier Material materials with Hardness, HBW of 360 [-]

Tensile strength

23.0 °C

800 - 1270 MPa

Show Supplier Material materials with Tensile strength of 800 - 1270 MPa

Yield strength

23.0 °C

520 - 1000 MPa

Show Supplier Material materials with Yield strength of 520 - 1000 MPa

Chemical properties

PropertyValueComment

Carbon

0.07 %

Show Supplier Material materials with Carbon of 0.07 %

Chromium

15 - 17.5 %

Show Supplier Material materials with Chromium of 15 - 17.5 %

Manganese

1 %

Show Supplier Material materials with Manganese of 1 %

Molybdenum

0.6 %

Show Supplier Material materials with Molybdenum of 0.6 %

Nickel

3 - 5 %

Show Supplier Material materials with Nickel of 3 - 5 %

Other

0.15 - 0.45 %

Show Supplier Material materials with Other of 0.15 - 0.45 %

Nb+Ta

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %