General
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.15 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.15 [-] | max. |
Dimension
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanical
Property | Value | Comment |
---|---|---|
Elongation | 33 % Show Supplier Material materials with Elongation of 33 % | min. | for thickness 1.8-2 mm | Transverse, A80 |
34 % Show Supplier Material materials with Elongation of 34 % | min. | for thickness 2-3 mm | Transverse, A80 | |
40 % Show Supplier Material materials with Elongation of 40 % | min. A5.65√So | for thickness 3-8 mm | Transverse | |
Tensile strength | 270 - 350 MPa Show Supplier Material materials with Tensile strength of 270 - 350 MPa | for thickness 1.8-8 mm | Transverse |
Yield strength | 180 - 290 MPa Show Supplier Material materials with Yield strength of 180 - 290 MPa | for thickness 1.8-2 mm | Transverse |
180 - 270 MPa Show Supplier Material materials with Yield strength of 180 - 270 MPa | for thickness 2-8 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | max. |
Carbon | 0.06 % Show Supplier Material materials with Carbon of 0.06 % | max. |
Manganese | 0.35 % Show Supplier Material materials with Manganese of 0.35 % | max. |
Phosphorus | 0.02 % Show Supplier Material materials with Phosphorus of 0.02 % | max. |
Silicon | 0.03 % Show Supplier Material materials with Silicon of 0.03 % | max. |
Sulfur | 0.02 % Show Supplier Material materials with Sulfur of 0.02 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | This is widely used for bending and drawing applications in general industry, building, the automotive industry and related sectors (e.g. oil sumps for industrial vehicles etc). ArcelorMittal's steels for cold forming and deep drawing applications display good or even excellent performance in all types of deep drawing processes, enabling the production of complex parts. Uncoated hot rolled steels for bending and deep drawing applications are suitable under certain conditions for food contact, as specified in the Regulation (EC) No. 1935/2004 and French standard NF A 36-714. Please contact us for further information on this subject. | |
Coating | Galvanisation: Class 1 | |
Other | ArcelorMittal provides guarantees for thicknesses greater than 11 mm. | |
Welding | The weldability (spot and arc welding) of ArcelorMittal's hot rolled steels for cold forming and deep drawing is equivalent to that of cold rolled steels of corresponding grades. |