General
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.4 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.4 [-] | max. |
Dimension
Property | Value |
---|---|
Dimensions | For mill finish, coils in thicknesses greater than 20 mm can also be produced. Please contact us. Please feel free to check the figure on the right side of the material page for more details. |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | -20 °C | 27 J Show Supplier Material materials with Charpy impact energy of 27 J | min. | for thickness 6-20 mm |
Elongation | 15 % Show Supplier Material materials with Elongation of 15 % | min. | for thickness 1.5-2 mm | Transverse, A80 | |
16 % Show Supplier Material materials with Elongation of 16 % | min. | for thickness 2-2.5 mm | Transverse, A80 | ||
17 % Show Supplier Material materials with Elongation of 17 % | min. | for thickness 2.5-3 mm | Transverse, A80 | ||
21 % Show Supplier Material materials with Elongation of 21 % | min. A5.65√So | for thickness 3-20 mm | Transverse | ||
Tensile strength | 410 - 560 MPa Show Supplier Material materials with Tensile strength of 410 - 560 MPa | for thickness 3-20 mm | Transverse | |
430 - 580 MPa Show Supplier Material materials with Tensile strength of 430 - 580 MPa | for thickness 1.5-3 mm | Transverse | ||
Yield strength | 265 MPa Show Supplier Material materials with Yield strength of 265 MPa | min. | for thickness 16-20 mm | Transverse | |
275 MPa Show Supplier Material materials with Yield strength of 275 MPa | min. | for thickness 1.5-16 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | min. |
Carbon | 0.18 % Show Supplier Material materials with Carbon of 0.18 % | max. |
Copper | 0.55 % Show Supplier Material materials with Copper of 0.55 % | max. |
Manganese | 1.5 % Show Supplier Material materials with Manganese of 1.5 % | max. |
Nitrogen | 0.012 % Show Supplier Material materials with Nitrogen of 0.012 % | max. |
Phosphorus | 0.025 % Show Supplier Material materials with Phosphorus of 0.025 % | max. |
Silicon | 0.03 % Show Supplier Material materials with Silicon of 0.03 % | max. |
Sulfur | 0.025 % Show Supplier Material materials with Sulfur of 0.025 % | max. |
Technological properties
Property | ||
---|---|---|
Chemical composition | The above chemical properties are based on cast analysis data. | |
Coating | Galvanisation: Class 1 |