Dimension
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.01 - 0.03 % Show Supplier Material materials with Aluminium of 0.01 - 0.03 % | |
Carbon | 0.65 - 0.73 % Show Supplier Material materials with Carbon of 0.65 - 0.73 % | |
Chromium | 0.2 - 0.3 % Show Supplier Material materials with Chromium of 0.2 - 0.3 % | |
Manganese | 0.6 - 0.75 % Show Supplier Material materials with Manganese of 0.6 - 0.75 % | |
Molybdenum | 0.08 % Show Supplier Material materials with Molybdenum of 0.08 % | max. |
Nickel | 0.1 % Show Supplier Material materials with Nickel of 0.1 % | max. |
Phosphorus | 0.025 % Show Supplier Material materials with Phosphorus of 0.025 % | max. |
Silicon | 0.15 - 0.25 % Show Supplier Material materials with Silicon of 0.15 - 0.25 % | |
Sulfur | 0.005 % Show Supplier Material materials with Sulfur of 0.005 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | It can be cold rolled and subjected to heat treatment (quenching and annealing), depending on its intended application, and is used to make mechanical parts, such as clutches, springs, segments, saw blades, measuring tape etc. | |
Delivery condtion | Other dimensions may be available after prior agreement. | |
Heat Treatment | As this steel grade generally undergo heat treatment, a number of diagrams showing typical behaviour is available on request, such as: | |
Other | Mechanical properties: Since this grade will undergo re-rolling or heat treatment, we cannot guarantee its mechanical properties when delivered. Please contact the supplier for further information on this subject. In view of the tolerance values required for finished products made from narrow strip, ArcelorMittal normally offers a tighter tolerance range for these grades (half the tolerance range required by the EN 10051:2010 standard). Transverse coil profile As this product is frequently re-rolled after slitting, ArcelorMittal can supply coils with an extra flat profile (to order), which can guarantee a hot-rolled strip crown lower than 60 µm for coil thicknesses ranging from 2 to 6 mm. Do not hesitate to contact us. Internal purity Our steels have the degree of internal purity corresponding to the steel grade specified. It is possible to agree on the required degree of purity at the time of enquiry and order. Decarburisation The guaranteed maximum decarburisation is 1% per side. |