Dimension
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanical
Property | Value | Comment |
---|---|---|
Bend allowance | 0 [-] Show Supplier Material materials with Bend allowance of 0 [-] | min. | Transverse | for thickness 0.5-3 mm |
Elongation | 19 % Show Supplier Material materials with Elongation of 19 % | min. | for thickness 0.5-0.7 mm | A80 | Transverse |
20 % Show Supplier Material materials with Elongation of 20 % | min. | for thickness 0.5-0.7 mm | A80 | |
21 % Show Supplier Material materials with Elongation of 21 % | min. | for thickness 0.7-3 mm | A80 | Transverse | |
22 % Show Supplier Material materials with Elongation of 22 % | min. | for thickness 0.7-3 mm | A80 | |
Tensile strength | 400 - 500 MPa Show Supplier Material materials with Tensile strength of 400 - 500 MPa | for thickness 0.5-3 mm |
410 - 510 MPa Show Supplier Material materials with Tensile strength of 410 - 510 MPa | for thickness 0.5-3 mm | Transverse | |
Yield strength | 320 - 410 MPa Show Supplier Material materials with Yield strength of 320 - 410 MPa | for thickness 0.5-3 mm |
340 - 420 MPa Show Supplier Material materials with Yield strength of 340 - 420 MPa | for thickness 0.5-3 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.015 % Show Supplier Material materials with Aluminium of 0.015 % | min. |
Carbon | 0.1 % Show Supplier Material materials with Carbon of 0.1 % | max. |
Manganese | 0.9 % Show Supplier Material materials with Manganese of 0.9 % | max. |
Niobium | 0.09 % Show Supplier Material materials with Niobium of 0.09 % | max. |
Phosphorus | 0.025 % Show Supplier Material materials with Phosphorus of 0.025 % | max. |
Silicon | 0.03 % Show Supplier Material materials with Silicon of 0.03 % | max. |
Sulfur | 0.02 % Show Supplier Material materials with Sulfur of 0.02 % | max. |
Titanium | 0.15 % Show Supplier Material materials with Titanium of 0.15 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The steel grade is particularly suitable for structural parts that do not require severe forming (profiling, bending or light drawing): automotive structures and reinforcements, industrial shelving systems, radiators, racking systems, furniture, mechanical engineering applications etc. | |
Coating | Galvanisation: Class 1 | |
Surface condition | Surface cleanliness If improved surface cleanliness is required, ArcelorMittal also offers this steel grade with compulsory use of continuous annealing or hydrogen annealing. | |
Welding | The steel grade has good weldability in all welding processes. Based on many years’ practical experience in arc and resistance spot welding of its products, ArcelorMittal can provide valuable technical assistance in defining the welding parameters for this grade. | |
Workability | Forming limit curves can be used to define the maximum strains not to be exceeded when forming steel by various methods, so as to avoid the risk of incipient necking. These curves are available on request. Please contact for other forming data on this grade for particular sheet thicknesses. |