General
Property | Value | Comment |
---|---|---|
Density | 7.75 g/cm³ Show Supplier Material materials with Density of 7.75 g/cm³ | for thickness 0.50 mm |
Mechanical
Property | Value | Comment |
---|---|---|
Elongation | 27 - 37 % Show Supplier Material materials with Elongation of 27 - 37 % | for thickness 0.50 mm | Transverse | A80 |
Hardness, Vickers | 135 - 165 [-] Show Supplier Material materials with Hardness, Vickers of 135 - 165 [-] | for thickness 0.50 mm |
Number of bends | 5 [-] Show Supplier Material materials with Number of bends of 5 [-] | min. for thickness 0.50 mm | Guaranteed |
Tensile strength | 420 - 470 MPa Show Supplier Material materials with Tensile strength of 420 - 470 MPa | for thickness 0.50 mm | Transverse |
Yield strength | 260 - 310 MPa Show Supplier Material materials with Yield strength of 260 - 310 MPa | for thickness 0.50 mm | Transverse |
Yield to strength ratio | 0.62 - 0.67 [-] Show Supplier Material materials with Yield to strength ratio of 0.62 - 0.67 [-] | for thickness 0.50 mm |
Magnetic
Property | Value | Frequency | Comment |
---|---|---|---|
Anisotropy of loss | 12 % Show Supplier Material materials with Anisotropy of loss of 12 % | (+/-) for thickness 0.50 mm | Guaranteed | |
Guaranteed core loss | 4 W/kg Show Supplier Material materials with Guaranteed core loss of 4 W/kg | 50Hz | max. for thickness 0.50 mm | at 1.5 T |
Guaranteed polarization | 1.62 [-] Show Supplier Material materials with Guaranteed polarization of 1.62 [-] | min. | for thickness 0.50 mm | at 2500 A/m | |
1.72 [-] Show Supplier Material materials with Guaranteed polarization of 1.72 [-] | min. | for thickness 0.50 mm | Indicative | ||
1.83 [-] Show Supplier Material materials with Guaranteed polarization of 1.83 [-] | min. | for thickness 0.50 mm | at 10000 A/m | ||
Stacking factor | 0.96 mm Show Supplier Material materials with Stacking factor of 0.96 mm | min. | for thickness 0.50 mm | Guaranteed | |
Typical core loss | 1.8 W/kg Show Supplier Material materials with Typical core loss of 1.8 W/kg | 50Hz | max. for thickness 0.50 mm | at 1 T |
5.1 W/kg Show Supplier Material materials with Typical core loss of 5.1 W/kg | 60Hz | max. for thickness 0.50 mm | at 1.5 T |
Technological properties
Property | ||
---|---|---|
Application areas | High permeability is particularly useful for applications such as ballasts and motors, because it makes it possible to build machines that meet the most stringent environmental regulations. High thermal conductivity is a significant advantage for large machines. | |
Coating | This high permeability grade is available non-insulated or varnished. | |
Other | The above properties are obtained without heat treatment after stamping. The material as supplied possesses all the required magnetic properties. |