General
Property | Value |
---|---|
Density | 7.65 g/cm³ Show Supplier Material materials with Density of 7.65 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elongation | 7 - 23 % Show Supplier Material materials with Elongation of 7 - 23 % | for thickness 0.50 mm | Transverse | A80 |
Hardness, Vickers | 150 - 210 [-] Show Supplier Material materials with Hardness, Vickers of 150 - 210 [-] | for thickness 0.50 mm |
Tensile strength | 450 - 550 MPa Show Supplier Material materials with Tensile strength of 450 - 550 MPa | for thickness 0.50 mm | Transverse |
Yield strength | 400 - 450 MPa Show Supplier Material materials with Yield strength of 400 - 450 MPa | for thickness 0.50 mm | Transverse |
Magnetic
Property | Value | Frequency | Comment |
---|---|---|---|
Guaranteed core loss | 3.4 W/kg Show Supplier Material materials with Guaranteed core loss of 3.4 W/kg | 50Hz | max. for thickness 0.50 mm | at 1 T |
Guaranteed polarization | 1.54 [-] Show Supplier Material materials with Guaranteed polarization of 1.54 [-] | min. | for thickness 0.50 mm | at 2500 A/m | |
1.62 [-] Show Supplier Material materials with Guaranteed polarization of 1.62 [-] | min. | for thickness 0.50 mm | at 5000 A/m | ||
1.72 [-] Show Supplier Material materials with Guaranteed polarization of 1.72 [-] | min. | for thickness 0.50 mm | at 10000 A/m | ||
Typical core loss | 1.42 W/kg Show Supplier Material materials with Typical core loss of 1.42 W/kg | 50Hz | max. for thickness 0.50 mm | at 1 T |
4.32 W/kg Show Supplier Material materials with Typical core loss of 4.32 W/kg | 60Hz | max. for thickness 0.50 mm | at 1.5 T |
Technological properties
Property | ||
---|---|---|
Application areas | Non-alloyed semi-processed electrical steels are designed for small industrial motors, fans and domestic appliances such as washing machine motors, microwave oven transformers and refrigerator compressors. Alloyed semi-processed electrical steels are designed for similar higher efficiency versions of these applications, as they have lower losses whilst the permeability remains at a good level. | |
Coating | This semi-processed grade is available non-insulated. The final process step in the decarburising annealing treatment carried out by the client provides a suitable atmosphere and thermal conditions for blueing: the formation of an oxide film, which creates the required surface insulation layer. | |
Other | The punching process needs to be carried out with an appropriate lubricant, which must be selected carefully, especially in the case of the alloyed semi-processed grades. |