Dimension
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanical
Property | Value | Comment |
---|---|---|
Elongation | 19 % Show Supplier Material materials with Elongation of 19 % | min. | for thickness 0.2-0.35 mm | Transverse | A80 |
22 % Show Supplier Material materials with Elongation of 22 % | min. | for thickness 0.35-5 mm | Transverse | A80 | |
24 % Show Supplier Material materials with Elongation of 24 % | min. | for thickness 0.5-7 mm | Transverse | A80 | |
26 % Show Supplier Material materials with Elongation of 26 % | min. | for thickness 0.7-3 mm | Transverse | A80 | |
Tensile strength | 270 - 420 MPa Show Supplier Material materials with Tensile strength of 270 - 420 MPa | for thickness 0.2-3 mm | Transverse |
Yield strength | 140 - 300 MPa Show Supplier Material materials with Yield strength of 140 - 300 MPa | for thickness 0.2-3 mm | Transverse | the Re-value only applies to skin-passed products (surface qualities B and C) |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbon | 0.12 % Show Supplier Material materials with Carbon of 0.12 % | max. |
Manganese | 0.6 % Show Supplier Material materials with Manganese of 0.6 % | max. |
Phosphorus | 0.1 % Show Supplier Material materials with Phosphorus of 0.1 % | max. |
Silicon | 0.5 % Show Supplier Material materials with Silicon of 0.5 % | max. |
Sulfur | 0.045 % Show Supplier Material materials with Sulfur of 0.045 % | max. |
Titanium | 0.3 % Show Supplier Material materials with Titanium of 0.3 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Galfan is used in numerous industrial applications, such as: | |
Coating | ||
Other | Storage Galvanised strips are usually supplied passivated or oiled to temporarily limit any risk of white rust formation. During transport and storage, all necessary precautions must be taken to keep the material dry and to prevent the formation of condensation. Improved protection can be achieved by the application of an Easyfilm® thin organic coating (please see data sheet E80 for the specific properties of Easyfilm®). Forming and joining The forming and joining techniques currently used for uncoated steel are also suitable for galvanised steel. It is essential to select a coating thickness that is compatible with the forming and joining processes envisaged, without compromising the desired degree of corrosion protection. Painting Hot dip galvanised steels can be painted after degreasing and surface treatment when supplied oiled. If an Easyfilm® thin organic coating has been applied, they can be painted directly, without any prior surface treatment. However, the paint must be compatible with the Easyfilm® resin. | |
Welding | In electrical resistance welding, the welding current must be suitably regulated and regularly adjusted. Electrode life can be extended by regularly stepping up the welding current and periodically dressing (machining) the electrodes. |