General
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.38 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.38 [-] | max. |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 0 °C | 24 J Show Supplier Material materials with Charpy impact energy of 24 J | min. | for thickness 5-50 mm | Transverse |
0 °C | 27 J Show Supplier Material materials with Charpy impact energy of 27 J | min. | for thickness 50-70 mm | Transverse | |
0 °C | 34 J Show Supplier Material materials with Charpy impact energy of 34 J | min. | for thickness 5-50 mm | |
0 °C | 34 J Show Supplier Material materials with Charpy impact energy of 34 J | min. | for thickness 70-100 mm | Transverse | |
0 °C | 41 J Show Supplier Material materials with Charpy impact energy of 41 J | min. | for thickness 50-70 mm | |
0 °C | 50 J Show Supplier Material materials with Charpy impact energy of 50 J | min. | for thickness 70-100 mm | |
Elongation | 21 % Show Supplier Material materials with Elongation of 21 % | min. A5.65√So | for thickness 5-100 mm | Transverse | |
Tensile strength | 490 - 630 MPa Show Supplier Material materials with Tensile strength of 490 - 630 MPa | for thickness 5-100 mm | Transverse | |
Yield strength | 355 MPa Show Supplier Material materials with Yield strength of 355 MPa | min. | for thickness 5-100 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | min. |
Carbon | 0.18 % Show Supplier Material materials with Carbon of 0.18 % | max. |
Chromium | 0.2 % Show Supplier Material materials with Chromium of 0.2 % | max. |
Copper | 0.35 % Show Supplier Material materials with Copper of 0.35 % | max. |
Manganese | 0.9 - 1.6 % Show Supplier Material materials with Manganese of 0.9 - 1.6 % | |
Molybdenum | 0.08 % Show Supplier Material materials with Molybdenum of 0.08 % | max. |
Nickel | 0.4 % Show Supplier Material materials with Nickel of 0.4 % | max. |
Nitrogen | 0.012 % Show Supplier Material materials with Nitrogen of 0.012 % | max. |
Other | 0.12 % Show Supplier Material materials with Other of 0.12 % | max. | Nb + Ti + V |
Phosphorus | 0.035 % Show Supplier Material materials with Phosphorus of 0.035 % | max. |
Silicon | 0.5 % Show Supplier Material materials with Silicon of 0.5 % | max. |
Sulfur | 0.035 % Show Supplier Material materials with Sulfur of 0.035 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Steel for shipbuilding can be used for the entire range of shipbuilding applications e.g. for the hull and interior of ships | |
Delivery condtion | For the dimensions available please visit Dimension tables (see Table A). | |
Other | Agreements The maximum thickness approved in shipbuilding specifications can be communicated on request by your sales agent. Available options Options available (after prior agreement): Mechanical properties Charpy V notch impact test specimens should be taken in the longitudinal direction. Transverse test specimens are not usually required. Transverse test results for plates and wide flats should be guaranteed by the supplier. |