PA66 GF30 black HAKAmid

Alternative and trade names
PA66-GF30, HAKAmid PA66 GF30 schwarz
Want to keep this datasheet? Save it now in your required format

Description

PA 66 standard viscosity, 30% glass fiber reinforced. Granulate contains recycled polymers coming from injection molding applications.

This material data has been provided by Aurora Kunststoffe GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

1.33 - 1.37 g/cm³

Show Supplier Material materials with Density of 1.33 - 1.37 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

7.5 - 8 GPa

Show Supplier Material materials with Elastic modulus of 7.5 - 8 GPa

ISO 527-2

Elongation

20.0 °C

3.2 - 3.8 %

Show Supplier Material materials with Elongation of 3.2 - 3.8 %

ISO 527-1/-2

Impact strength, Charpy notched

20.0 °C

7 - 11 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 7 - 11 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

20.0 °C

40 - 60 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 40 - 60 kJ/m²

ISO 179/1eA

Tensile strength

20.0 °C

120 - 140 MPa

Show Supplier Material materials with Tensile strength of 120 - 140 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValue

Ash content

20.0 °C

28 - 32 %

Show Supplier Material materials with Ash content of 28 - 32 %

Rheological Properties

PropertyValueComment

Melt volume-flow rate

40 - 80 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 40 - 80 cm³/10min

ISO 1133, 275°C/5Kg

Technological properties

Property
Application areas

Cable protection parts for vehicles, Cable ties, Electrical and electronic application, Acoustic components, Cable ducts, brackets in the automotive sector, covers, frames, Reinforcing elements, Radiator cowl, Gear lever housing, Fans / Frames, Parts for furniture and chair industry

Fillers

30% Glass Fiber

Processing methods

Pre-drying 2-4 hours/80°C