Aluminium Oxide with 96% purity and the following features:


  • Electrical insulation
  • Thermal resistance
  • Resistance to thermal shock
  • Hardness
  • Pressure resistance
  • This material data has been provided by Bosch Advanced Ceramics.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    3.8 g/cm³

    Show Supplier Material materials with Density of 3.8 g/cm³

    Surface roughness

    5.1 μm

    Show Supplier Material materials with Surface roughness of 5.1 μm

    Rz*

    Mechanical

    PropertyTemperatureValueComment

    Compressive strength

    23.0 °C

    2800 MPa

    Show Supplier Material materials with Compressive strength of 2800 MPa

    Elastic modulus

    23.0 °C

    340 GPa

    Show Supplier Material materials with Elastic modulus of 340 GPa

    Flexural strength

    23.0 °C

    400 MPa

    Show Supplier Material materials with Flexural strength of 400 MPa

    4-point bending flexural test

    Hardness, Vickers

    23.0 °C

    1428 [-]

    Show Supplier Material materials with Hardness, Vickers of 1428 [-]

    converted from GPa

    Plane-Strain Fracture Toughnes

    23.0 °C

    4.2 MPa·√m

    Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4.2 MPa·√m

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    23.0 °C

    8E-6 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 8E-6 1/K

    Thermal conductivity

    23.0 °C

    24 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 24 W/(m·K)

    Electrical

    PropertyTemperatureValue

    Electrical resistivity

    20.0 °C

    1.00E+14 Ω·m

    Show Supplier Material materials with Electrical resistivity of 1.00E+14 Ω·m

    600.0 °C

    1000000 Ω·m

    Show Supplier Material materials with Electrical resistivity of 1000000 Ω·m

    Technological properties

    Property
    Application areas

    Wear parts for the textile and the machine engineering industry

    Suitable for high temperatures and corrosive environments, e.g. in laboratories

    Insulating parts for electronics and electrical engineering

    Other

    *depending on the processing status of the injection molding or pressing tool

    Processing history