Description

Alloy 286 is a precipitation hardened austenitic iron based steel, suitable for applications requiring high strength, good corrosion resistance at temperatures up to 700 degree C, and a high degree of uniformity in developing full strength.

Related Standards

Equivalent Materials

This material data has been provided by Broder Metals Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Length

12.7 - 127 mm

Show Supplier Material materials with Length of 12.7 - 127 mm

Mechanical

PropertyTemperatureValueComment

Creep strength

650.0 °C

385 MPa

Show Supplier Material materials with Creep strength of 385 MPa

For 100 hours resulting in 5% elongation

Elongation

23.0 °C

15 %

Show Supplier Material materials with Elongation of 15 %

Hardness, Brinell

23.0 °C

248 - 321 [-]

Show Supplier Material materials with Hardness, Brinell of 248 - 321 [-]

Hardness, Rockwell C

23.0 °C

29 - 35 [-]

Show Supplier Material materials with Hardness, Rockwell C of 29 - 35 [-]

Reduction of area

23.0 °C

18 %

Show Supplier Material materials with Reduction of area of 18 %

Tensile strength

23.0 °C

895 MPa

Show Supplier Material materials with Tensile strength of 895 MPa

Yield strength Rp0.2

23.0 °C

725 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 725 MPa

Chemical properties

PropertyValue

Aluminium

0.3 - 0.4 %

Show Supplier Material materials with Aluminium of 0.3 - 0.4 %

Boron

0.0001 - 0.01 %

Show Supplier Material materials with Boron of 0.0001 - 0.01 %

Carbon

0.07 - 0.09 %

Show Supplier Material materials with Carbon of 0.07 - 0.09 %

Chromium

13.5 - 16 %

Show Supplier Material materials with Chromium of 13.5 - 16 %

Iron

Balance

Manganese

1.96 - 2.04 %

Show Supplier Material materials with Manganese of 1.96 - 2.04 %

Molybdenum

1 - 1.5 %

Show Supplier Material materials with Molybdenum of 1 - 1.5 %

Nickel

24 - 27 %

Show Supplier Material materials with Nickel of 24 - 27 %

Phosphorus

0.04 - 0.05 %

Show Supplier Material materials with Phosphorus of 0.04 - 0.05 %

Silicon

0.95 - 1.05 %

Show Supplier Material materials with Silicon of 0.95 - 1.05 %

Sulfur

0.025 - 0.035 %

Show Supplier Material materials with Sulfur of 0.025 - 0.035 %

Titanium

1.9 - 2.35 %

Show Supplier Material materials with Titanium of 1.9 - 2.35 %

Vanadium

0.1 - 0.5 %

Show Supplier Material materials with Vanadium of 0.1 - 0.5 %

Technological properties