Description

Produced via Electric Arc / Electric + AOD

Related Standards

Equivalent Materials

This material data has been provided by Broder Metals Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

16 %

Show Supplier Material materials with Elongation of 16 %

Hardness, HBW

23.0 °C

335 [-]

Show Supplier Material materials with Hardness, HBW of 335 [-]

Hardness, Rockwell C

23.0 °C

36 [-]

Show Supplier Material materials with Hardness, Rockwell C of 36 [-]

Tensile strength

23.0 °C

860 MPa

Show Supplier Material materials with Tensile strength of 860 MPa

Chemical properties

PropertyValue

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

Chromium

24 - 26 %

Show Supplier Material materials with Chromium of 24 - 26 %

Copper

0.5 - 1 %

Show Supplier Material materials with Copper of 0.5 - 1 %

Iron

Balance

Manganese

1 %

Show Supplier Material materials with Manganese of 1 %

Molybdenum

3 - 4 %

Show Supplier Material materials with Molybdenum of 3 - 4 %

Nickel

6 - 8 %

Show Supplier Material materials with Nickel of 6 - 8 %

Nitrogen

0.2 - 0.3 %

Show Supplier Material materials with Nitrogen of 0.2 - 0.3 %

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

Sulfur

0.01 %

Show Supplier Material materials with Sulfur of 0.01 %

Tungsten

0.5 - 1 %

Show Supplier Material materials with Tungsten of 0.5 - 1 %

Technological properties

Property
Corrosion properties

Stress Corrosion: material is tested in accordance with ASTM G48 (Method A) (latest version). The test piece will be taken from the same location as those for mechanical testing. Acceptance is that no pitting is to be observed at 20x magnification after exposure for 24 hours at 50 degrees C. Weight loss will not exceed 4.0 g/mm2. Method and results are reported.