General

PropertyTemperatureValue

Density

23.0 °C

8.87 g/cm³

Show Supplier Material materials with Density of 8.87 g/cm³

Dimension

PropertyValue

Diameter

10 - 250 mm

Show Supplier Material materials with Diameter of 10 - 250 mm

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

40 %

Show Supplier Material materials with Elongation of 40 %

Hardness, HBW

23.0 °C

325 [-]

Show Supplier Material materials with Hardness, HBW of 325 [-]

Hardness, Rockwell C

23.0 °C

35 [-]

Show Supplier Material materials with Hardness, Rockwell C of 35 [-]

Tensile strength

23.0 °C

690 MPa

Show Supplier Material materials with Tensile strength of 690 MPa

Yield strength Rp0.2

23.0 °C

283 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 283 MPa

Chemical properties

PropertyValue

Carbon

0.01 %

Show Supplier Material materials with Carbon of 0.01 %

Chromium

14.5 - 16.5 %

Show Supplier Material materials with Chromium of 14.5 - 16.5 %

Cobalt

2.5 %

Show Supplier Material materials with Cobalt of 2.5 %

Iron

4 - 7 %

Show Supplier Material materials with Iron of 4 - 7 %

Manganese

1 %

Show Supplier Material materials with Manganese of 1 %

Molybdenum

15 - 17 %

Show Supplier Material materials with Molybdenum of 15 - 17 %

Nickel

Balance

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

0.08 %

Show Supplier Material materials with Silicon of 0.08 %

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %

Tungsten

3 - 4 %

Show Supplier Material materials with Tungsten of 3 - 4 %

Vanadium

0.35 %

Show Supplier Material materials with Vanadium of 0.35 %

Technological properties

Property
Application areas

Alloy C276 can be used in the most severe environments such as chemical and petrochemical processing involving bleach, pollution control, pulp and paper production, industrial and municipal waste treatment, pharmaceutical and food processing equipment, and process plant involved in the recovery of sour natural gas. Alloy C276 is ideal for use in evaporators, heat exchangers, sulphuric acid filters and reactors, and process plant handling acid catalysts.

Corrosion properties

C276 is resistant to pitting, stress corrosion cracking, and crevice corrosion in a wide range of chemical environments, particularly in chloride gas, hypochlorite and chlorine dioxide solutions. Meanwhile the chromium content adds resistance to oxidizing media, such as ferric and cupric chlorides. To complete the overall corrosion resisting properties, tungsten is present to provide additional general resistance in a wide range of severe environments.

Welding

Welding properties are good, with the low carbon content minimizing carbide / grain boundary precipitation during welding to maintain corrosion resistance in the welded finished condition.