Description

Alloy 400 is a nickel-copper alloy that is resistant to sea water and steam at elevated temperatures.

Related Standards

Equivalent Materials

This material data has been provided by Broder Metals Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Diameter

12.7 - 250 mm

Show Supplier Material materials with Diameter of 12.7 - 250 mm

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

180 GPa

Show Supplier Material materials with Elastic modulus of 180 GPa

Elongation

23.0 °C

45 %

Show Supplier Material materials with Elongation of 45 %

Tensile strength

23.0 °C

520 MPa

Show Supplier Material materials with Tensile strength of 520 MPa

Yield strength Rp0.2

23.0 °C

240 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 240 MPa

Chemical properties

PropertyValue

Aluminium

0.5 %

Show Supplier Material materials with Aluminium of 0.5 %

Carbon

0.3 %

Show Supplier Material materials with Carbon of 0.3 %

Iron

2.5 %

Show Supplier Material materials with Iron of 2.5 %

Manganese

2 %

Show Supplier Material materials with Manganese of 2 %

Nickel

63 - 70 %

Show Supplier Material materials with Nickel of 63 - 70 %

Silicon

0.5 %

Show Supplier Material materials with Silicon of 0.5 %

Sulfur

0.24 %

Show Supplier Material materials with Sulfur of 0.24 %

Technological properties

Property
Application areas

Valves, Fasteners and Marine engineering, Chemical and hydrocarbon processing equipment, Pumps, Propeller shafts, Oil and fresh water tanks, Fittings, Heat exchangers