Description

SKYi Stabil-MH5106 is a special heat stabilized long glass fibre reinforced polyamide grade, for injection moulding and extrusion. The long glass fibres, chemically coupled to the polyamide matrix, providing outstanding mechanical properties. SKYi Stabil-MH5106 is available both in black and natural. Other colours can be provided on request.

This material data has been provided by BUFA.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

1.54 g/cm³

Show Supplier Material materials with Density of 1.54 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

17 GPa

Show Supplier Material materials with Elastic modulus of 17 GPa

ISO 527-I

Elongation

20.0 °C

2.1 %

Show Supplier Material materials with Elongation of 2.1 %

ISO 527-I

Flexural modulus

20.0 °C

15.2 GPa

Show Supplier Material materials with Flexural modulus of 15.2 GPa

ISO 178

Flexural strength

20.0 °C

355 MPa

Show Supplier Material materials with Flexural strength of 355 MPa

ISO 178

Impact strength, Charpy notched

20.0 °C

35 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 35 kJ/m²

ISO 179-I

Tensile strength

20.0 °C

240 MPa

Show Supplier Material materials with Tensile strength of 240 MPa

ISO 527-I

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

230 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 230 °C

ISO 75-I

Technological properties

Property
Application areas

SKYi Stabil-MH5106 is intended for injection moulding of highly demanding technical applications.

The excellent properties of SKYi Stabil-MH5106 make it suitable for: Electrical components, automotive parts, interior, exterior and under the bonnet, structural furniture parts, load bearing, demanding components for various engineering sectors.

SKYi Stabil-MH5106 can, in many of these applications, substitute other engineering plastics or metal alloys.

Color

Available both in black and natural. Other colours can be provided on request.

Other

Safety: SKYi Stabil-MH5106 is not classified as a dangerous preparation.

Dust and fines from the product may give a risk for dust explosion. All equipment should be properly earthed. Inhalation of dust may irritate the respiratory system and should be avoided. During processing of the product small amounts of fumes are generated, which require proper ventilation.


Recycling: The product is suitable for recycling using modern methods of shredding and cleaning. Inhouse production waste should be kept clean to facilitate direct recycling. A Materials Safety Data Sheet is available on request. Please contact your SKYi representative for more details on various aspects of safety, recovery and disposal of the product.

Processing methods

Injection Molding:

Feed section (°C)Nozzle (°C)Melt temperature (°C)Mold temperature (°C)
240-250260-270270-28090-100