General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.5 g/cm³ Show Material materials with Density of 7.5 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 10 - 12 % Show Material materials with Elongation of 10 - 12 % |
Tensile strength | 23.0 °C | 650 - 700 MPa Show Material materials with Tensile strength of 650 - 700 MPa |
Yield strength Rp0.2 | 23.0 °C | 320 - 400 MPa Show Material materials with Yield strength Rp0.2 of 320 - 400 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K | for 0-300°C |
Melting point | 1060 - 1075 °C Show Material materials with Melting point of 1060 - 1075 °C | ||
Thermal conductivity | 23.0 °C | 59 - 67 W/(m·K) Show Material materials with Thermal conductivity of 59 - 67 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 6.96E+6 - 8.12E+6 S/m Show Material materials with Electrical conductivity of 6.96E+6 - 8.12E+6 S/m |
Specific Electrical conductivity | 12 - 14 % IACS Show Material materials with Specific Electrical conductivity of 12 - 14 % IACS |
Magnetic
Property | Temperature | Value |
---|---|---|
Relative magnetic permeability | 23.0 °C | 1.5 [-] Show Material materials with Relative magnetic permeability of 1.5 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 8.5 - 11 % Show Material materials with Aluminium of 8.5 - 11 % | ||
Copper | Balance | ||
Iron | 4 - 5.5 % Show Material materials with Iron of 4 - 5.5 % | ||
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % | max. | |
Nickel | 4 - 5.5 % Show Material materials with Nickel of 4 - 5.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Valve and pump components, marine hardware and high strength fasteners;Aerospace: High strength fasteners, springs, thrust washers and bearing bushes;Other: Gears, bearing races, valve stems, valve seats, worm gears, bearings, bushes, cams, pump rods and safety tools | |
Corrosion properties | Very high resistance to erosion and corrosion |