NIBRON SPECIAL® is an extra high strength copper nickel alloy developed by Columbia Metals that maximises both strength and corrosion resistance. Sometimes referred to as a nickel bronze, NIBRON® contains additions of aluminium, iron and manganese that join with the copper and nickel to achieve its exceptional properties. The resulting high strength, outstanding corrosion resistance, low magnetism, anti-galling, high conductivity and good fabrication characteristics combine to create a material suited to widely differing industries.

Related Standards

Equivalent Materials

Properties

General

Density ρ

8.5 g/cm³ at 20 °C

Mechanical

Elastic modulus E

141 GPa at 20 °C

Elongation A

12 % at 20 °C

Hardness, Brinell HB

229 - 240 [-] at 20 °C

Tensile strength Rm

770 - 850 MPa at 20 °C

Yield strength YS

555 - 630 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.64E-5 1/K at 20 °C

Melting point Tm

1080 - 1100 °C

Thermal conductivity λ

44 - 46 W/(m·K) at 20 °C

Electrical

Electrical resistivity ρel

1.7E-7 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

-

REM

Ni

14.5 %

Al

3 %

Fe

1.5 %

Mn

0.3 %

This material data has been provided by Columbia Metals.