General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.77 g/cm³ Show Supplier Material materials with Density of 2.77 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 240 GPa Show Supplier Material materials with Elastic modulus of 240 GPa |
Flexural strength | 23.0 °C | 180 MPa Show Supplier Material materials with Flexural strength of 180 MPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 3.2 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3.2 MPa·√m |
Poisson's ratio | 23.0 °C | 0.2 [-] Show Supplier Material materials with Poisson's ratio of 0.2 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1000.0 °C | 4E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4E-6 1/K | |
Max service temperature | 1500 °C Show Supplier Material materials with Max service temperature of 1500 °C | in inert gas | |
Max service temperature, long | 1500 °C Show Supplier Material materials with Max service temperature, long of 1500 °C | in air | |
Thermal conductivity | 23.0 °C | 23 W/(m·K) Show Supplier Material materials with Thermal conductivity of 23 W/(m·K) | |
Thermal shock parameter R1 | 150 °C Show Supplier Material materials with Thermal shock parameter R1 of 150 °C | ||
Thermal shock parameter R2 | 3450 W/m Show Supplier Material materials with Thermal shock parameter R2 of 3450 W/m |